Sibur MPP 21015-E10 Frost Resistant Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures
| Available Properties |
- Melt Index of Compound
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact Unnotched
- Vicat Softening Point
- Frost Resistance
|
|
|
|