Sibur Discar-L PC/ABS Compositional Polymer
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic
Material Notes: Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for structural parts of technical purpose and parts for internal finishing of automobiles.