Sibur KF-MT-15 Carbamide Formaldehyde Resin
Subcategory: Thermoplastic
Material Notes: In binding materials for production of wood laminate, base of glues for wood materials, for impregnation of paper during production of synthetic veneer sheet, production of varnish, production of rods and forms in the metallurgical industry. Mixing of resin with water in ratio of 2:1-1:10 where there is coagulation in volume.
| Available Properties |
- Viscosity Measurement
- Gel Time
- Concentration of Hydrogen Ions
- Mass Fraction of Dry Residue
- Mass Fraction of Free Formaldehyde
- Mass Share of Water
- Ultimate Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|