Sibur BSK-1904 B Styrene-Butadiene Rubber (SBR)
Subcategory: Elastomer, TS; Thermoset
Material Notes: HSK-1904. For production of sole rubbers, artificial leather, and rubber technical articles.
| Available Properties |
- Ash
- Loss During Drying
- Mass Share of A-Methyl Styrene
- Mass Share of Vingstay T
- Non-Polymerized Styrene and A-Methyl Styrene
- Spread Flow Batch Error
|
|
|
|