Sibur Nitrilast-40 Nitrile-Butadiene Rubber (NBR)
Subcategory: Elastomer, TS; Thermoset
Material Notes: N 3883. For production of oil-benzene resistant articles for the automobile, aviation and rubber technical industries. Rubbers on the base of Nitrilast possess good oil-benzene resistance. Rubber mixtures on the base of Nitrilast are more resistant to wearing than those made of natural rubber.
| Available Properties |
- Mooney Viscosity
- Ash
- Tensile Strength at Break
- Elongation at Break
- Loss During Drying
- Mass Share Adigol-2
- Mass Share of VS-30A
|
|
|
|