SIDPEC EGYPTENE® HD 4602 FA, HDPE Film
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Material Notes: Applications:- Strong film
- Trash bag
- Shopping bag
Film properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height. Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Dart Drop
- Dart Drop Test
|
|
|
|
| Property Data |