SIDPEC EGYPTENE® LL 0205 AF, LLDPE Film
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Applications:- Heavy duty sacks, mulch films
- Stretch film, liners, geomembrane
Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1. Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Dart Drop Test
- Vicat Softening Point
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|