SIDPEC EGYPTENE® HD 5301 EA, HDPE Blow Molding
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Applications:- High performance blow molded containers typically of to 60 liters capacity for packaging aggressive products
- Robust industrial and technical moldings
Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
| Available Properties |
- Density
- ESCR, Bottle
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Impact
|
|
|
|
| Property Data |