Sika 201 SikaFlex Adhesive
Subcategory: Adhesive; Thermoset
Material Notes: Sika 201 SikaFlex Adhesive Sikaflex 201 meets Federal Specification TT-S-00230C, Type II, Class A and ASTK C-920, Type S, Grade NS. 15 - 15 mm Cut-Off. Good non-sag. Available in black, white, gray, tan, MB bronze. Cure Type: Moisture
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Adhesive Bond Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Cure Time
- Shelf Life
|
|
|
|