Sika 219 LM SikaFlex Low Modulus Polyurethane Sealant
Subcategory: Adhesive; Polyurethane, TS; Thermoset
Material Notes: Sika 219 LM SikaFlex Low Modulus Polyurethane Sealant This is a high performance, low modulus polyurethane base, non-sag elastomeric sealant with excellent adhesion to a wide variety of substrates. Meets Federal Specification TT-S-00230C, Type II, Class A and ASTM C-920, Type S, Grade NS, Class 25 and TT-S-001543A, Type non-sag. 12 - 15 mm Cut-Off. Excellent non-sag. Available in black, white, gray, tan, MB bronze, limestone. Cure Type: Moisture
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Adhesive Bond Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|