Simrit 70 Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of elasticity. Simriz® perfluoro elastomers close the material gap between inelastic PTFE and elastomers, which have poor temperature and chemical resistance properties. With a fluoridation level of 72%, FFKM elastomers have a level of resistance close to that of pure PTFE at 76%. At the same time, FFKM materials are so elastic that they are excellently suited to both static and dynamic seals. Simrit offers ISC O-Rings which are specifically optimised with respect to flexibility at low temperatures, resistance to high temperatures, hardness, tensile strength, elongation, compression set, or color. Information provided by Freudenburg-NOK.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Compression Set, Elevated Temperature
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
- Water Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|