Simrit Low Temperature Polyurethane Elastomer 92 AU 21100
Subcategory: Elastomer, TS; Polyurethane, TS; Thermoset
Material Notes: With the new low temperature material 92 AU 21100, Simrit has succeeded in developing a polyurethane material that is specially designed to meet the specific requirements for use at low temperatures and yet can also handle standard applications with no problems: the operating range of 92 AU 21100 stretches from –50 to +100°C. This is made possible by targeted modification of the PU components responsible for temperature properties, while leaving the remaining material properties comparable to Simrit’s standard PU materials. The 92 AU 21100 PU material demonstrates particularly beneficial viscoelastic behaviour, whereby the soft segments retain their flexibility over a broad range of temperatures and only solidify at very low temperatures. There is no negative influence on other critical material properties such as hardness and tensile strength. In practical terms, this means that seals made of the 92 AU 21100 material are sufficiently flexible even at extremely low temperatures and have the necessary sealing effect immediately after commissioning. This allows initial leakages to be reliably prevented. Information provided by Freudenburg-NOK.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Resilience
- Compression Set
- Compression Set, Elevated Temperature
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- TR 10
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|