SKYGREEN® PETG 2008, Specially Formulated PET Copolymer Resin
Subcategory: Polyethylene; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Description: SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processability and clarity. Skygreen® PETG provides a material having outstanding toughness, clarity, color, chemical resistance, and resistance to stress whitening. It can readily be thermoformed for extrusion blow molded. It is superior to acrylic for toughness, and superior to polycarbonate for processability. Applications: Extrusion Sheet: architecture protective cover, display signs, industrial products. Extrusion Film: blister packaging, food packaging containers, electrical & electronic packaging, pharmaceutical & medical packaging. Injection Molding: toys, refrigerator parts, electric & electronic parts, smart cards, pen caps, medical devices and tools. Extrusion Blow Molding: bottles for cosmetics, soaps, shampoos, detergents, etc. Information provided by SK Chemicals.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Impact Test
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
- Processing Temperature
- Feed Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Zone 5
- Adapter Temperature
- Die Temperature
- Head Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Hold Pressure
- Back Pressure
- Cycle Time - Injection
- Cycle Time - Cooling
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|