SKYPET® - BL8450, Specially Formulated PET Copolymer Resin
Subcategory: Polyethylene; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Description: SKYPET-BL8450 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8450 provides excellent processability in injection molding and blow molding processes, offers low Acetaldehyde contents (max 1 ppm) in the final container, has excellent thermal stability during melt processing, has slower crystallization rate suitable for highly transparent container. Applications: Carbonated soft drink bottles, mineral water bottles, custom bottles, extruded sheet and thermoformed articles. Information provided by SK Chemicals.
| Available Properties |
- Density
- Bulk Density
- Viscosity Test
- Melting Point
- Moisture Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|