SKYTHANE UB220, Ink Binder
Subcategory: Elastomer, TPE; Polyurethane, TP; Additive/Filler for Polymer; Thermoplastic
Material Notes: Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic tapes and inks, adhesives for shoe industries and PVC lamination, etc. UB series have good solubility to various kinds of industrial solvents and cover a wide range of solution viscosity.Information provided by SK Chemicals.