SKYTHANE US518, Adhesive (Dry Lamination)
Subcategory: Elastomer, TPE; Adhesive; Polyurethane, TP; Thermoplastic
Material Notes: Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:- Keyboard Covers
- Outsoles of Soccer Shoes
- Wire and Cable
- Airbags
- Sheets and Film
- Hoses and Tubing
- Shoe Components
- Fire Hoses
Information provided by SK Chemicals.
| Available Properties |
- Solids Content
- Viscosity
- Molecular Weight
- Glass Temperature
- Appearance
|
|
|
|