SK chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been developed on the basis of the SK Chemicals polyethylene terephthalate (PET) technology. There is no other chemical linkage than ester in its molecular structure. SkyGreen fully degrades into CO2 and H2O via hydrolysis mechanism. Within 45 days, the polymer degrades completely in the composting condition. Information provided by SK Chemicals
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|