Turcite® TX Self-Lubricating Thermoplastic Rod
Subcategory: Thermoplastic; Polymer; ; ; ; ; ; ; ; ;
Key Words: Busak + Shamban; TI Group; Smiths Group
Material Notes: Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coefficient of friction and high PV. General Turcite® information: Exhibit excellent wear resistance, durability, and no slip-stick under oscillating motion. Axial-loaded shafts benefit from reduced friction. Uses include transmissions, home appliances, bicycles, food processing equipment, exercise equipment, rotating displays, and caster assemblies. Informatiuon provided by Busak + Shamban, now a subsidiary of Smiths Group
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|