Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer

 

Subcategory: Ethylene Vinyl Alcohol; Thermoplastic

Key Words: EVOH

Material Notes:
Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.

The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a thin gas barrier layer without loss of shelf life.

Soarnol DT2903 with low melt flow index is one of the standard grade of Soarnol, its ethylene content is 29 mol%. Since Soarnol DT2903 has a good gas barrier at low humidity, this resin is suited for coextruded film and coextrusion coating. This resin can also be used in coextruded sheet, coextruded blow-molded containers and coextruded inflation film.

Processing: Extruder:40 m screw type, L/D=28;Screw:Full-flighted, constant pitch type, CR=4.0;Screen pack:80/120/50 mesh;Die:Manifold type, die width=450 mm, lip distance=0.2 mm.

Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex,L.L.C., an affiliate of Nippon Gohsei.

Available Properties
  • Density
  • Moisture Vapor Transmission
  • Oxygen Transmission
  • Viscosity
  • Melt Flow
  • Melting Point
  • Crystallization Temperature
  • Glass Temperature
  • Refractive Index
  • Nozzle Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。