Soarnol® DC3203F Ethylene Vinyl Alcohol Copolymer
Subcategory: Ethylene Vinyl Alcohol; Thermoplastic
Key Words: EVOH
Material Notes: Low ethylene content. Suitable for use in packaging material used at normal temperature and humidity. Ethylene content 32 mol%. Volatile matter 0.3%. Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Viscosity
- Melt Flow
- Melting Point
- Crystallization Temperature
- Glass Temperature
- Refractive Index
- Haze
- Nozzle Temperature
|
|
|
|