Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer
Subcategory: Ethylene Vinyl Alcohol; Thermoplastic
Key Words: EVOH
Material Notes: Ethylene content 44 mol%. Volatile matter 0.3%. The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a thin gas barrier layer without loss of shelf life. Soarnol A4412 with high melt flow index is one of the standard grade of Soarnol, its ethylene content is 44 mol%. Soarnol A4412 has excellent water resistance and has a gas barrier property that does not drastically lower at high humidity, so Soarnol A4412 can be used as the most outer layer of multi layer film. This resin suited for coextruded film and coextruded pipe. Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Viscosity
- Melt Flow
- Melting Point
- Crystallization Temperature
- Glass Temperature
- Refractive Index
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|