Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer
Subcategory: Ethylene Vinyl Alcohol; Thermoplastic
Key Words: EVOH
Material Notes: Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%. The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a thin gas barrier layer without loss of shelf life. Soarnol BG3522 has gas barrier and high flow property. This grade is suited for extrusion coating. Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Viscosity
- Melt Flow
- Melting Point
- Crystallization Temperature
- Glass Temperature
- Refractive Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|