Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer
Subcategory: Ethylene Vinyl Alcohol; Thermoplastic
Key Words: EVOH
Material Notes: Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%. The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a thin gas barrier layer without loss of shelf life. Soarnol BS3803 has excellent stretchability without lower of gas barrier property. This grade is appropriate to co-extrusion and co-stretching with polypropylene. Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Viscosity
- Melt Flow
- Melting Point
- Crystallization Temperature
- Glass Temperature
- Refractive Index
- Haze
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|