Solvay Advanced Polymers Supradel® HTS-2420 High Temperature Sulfone Resin

 

Subcategory: Polysulfone; Thermoplastic

Close Analogs:

Supradel® has been replaced by EpiSpire™. Please see current data under that trade name.

Material Notes:
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. This resin represents a technological breakthrough as it defines a new benchmark in amorphous thermoplastics thermal performance capabilities available to today’s design engineers. With a glass transition temperature of 245°C and a heat deflection temperature of 240°C, SUPRADEL HTS-2420 resin this resin extends the thermal capability range available to design engineers today in other commercially available sulfone polymers (polysulfone, polyethersulfone and polyphenylsulfone).

The resin is completely amorphous and fully thermoplastic allowing easy melt fabrication by means of operations such as injection molding and extrusion. Along with its high thermal performance capabilities, SUPRADEL HTS-2420 resin also has a long list of high-performance attributes which include excellent hydrolytic stability, resistance to acids and bases, and inherent flame retardance.

SUPRADEL HTS-2420 resin is easily amenable to fabrication by injection molding, and other thermoplastic fabrication techniques. By virtue of its very high temperature performance and the unique combination of other engineering attributes, SUPRADEL HTS-2420 resin constitutes a good candidate for metal replacement as well as non-thermoplastic resin replacement in a wide range of engineering applications.

SUPRADEL HTS-2420 resin is available in natural and black.

Information provided by Solvay Advanced Polymers

Available Properties
  • Specific Gravity
  • Water Absorption
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Melt Flow
  • Tensile Strength @ Break
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。