MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Solvay Advanced Polymers Supradel® HTS-2400 High Temperature Sulfone Resin

 

Subcategory: Polysulfone; Thermoplastic

Close Analogs:

Supradel® has been replaced by EpiSpire™. Please see current data under that trade name.

Material Notes:
SUPRADEL HTS-2400 is a new high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the thermal capability range available to design engineers today in other commercially available sulfone polymers (polysulfone, polyethersulfone and polyphenylsulfone).

The resin is completely amorphous and fully thermoplastic allowing easy melt fabrication by means of operations such as injection molding and extrusion. Along with its high thermal performance capabilities, SUPRADEL HTS-2400 resin also has a long list of high-performance attributes which include excellent hydrolytic stability, resistance to acids and bases, and inherent flame retardance.

The ease of melt fabrication, coupled with the completely amorphous character assures tight dimensional control during injection molding of precision parts and components. The versatile performance profile of SUPRADEL HTS-2400 resin makes it a good candidate for metal replacement or the replacement of difficult-to-process thermoplastics in a wide range of engineering applications.

In its natural state, Supradel HTS-2400 resin is transparent with an amber color.

Information provided by Solvay Advanced Polymers

Available Properties
  • Specific Gravity
  • Water Absorption
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Melt Flow
  • Tensile Strength @ Break
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  • Refractive Index
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。