Solvay Advanced Polymers AvaSpire™ AV-750 GF40 NT Modified PEEK Resin, 40% Glass Reinforced
Subcategory: Polyetheretherketone (PEEK); Thermoplastic; Polymer
Material Notes: AvaSpire AV-750 GF40 NT resin was developed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone) system. This modified PEEK is 40% glass reinforced and provides the typical chemical resistance expected of PEEK while maintaining excellent elevated temperature properties.The price and performance of this resin will expand the opportunities for PEEK resins especially in the area of metal replacement for corrosion control. AvaSpire AV-750 GF40 NT resin can be easily processed on conventional injection molding equipment. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Water Absorption
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Yield Strength
- Shear Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|