Solvay Advanced Polymers AvaSpire™ AV-650 GF30 Modified PEEK, 30% Glass Reinforced
Subcategory: Polyetheretherketone (PEEK); Thermoplastic; Polymer
Material Notes: AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced, modified PEEK (polyetheretherketone) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength and stiffness than unfilled AV-650 resin. This material can be repeatedly exposed to harsh chemicals and prolonged steam sterilization cycles without any significant loss of properties, and it is USP Class VI compliant. The resin is designed to offer performance comparable to that of glass-reinforced PEEK while generally affording superior economics.Typical potential applications for this resin include orthopedic and dental instruments, surgical power tool battery housings and other devices and components requiring a combination of high temperature performance and high environmental resistance. AvaSpire AV-650 GF30 can be easily processed by typical injection molding and extrusionmethods using standard equipment. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Water Absorption
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|