Solvay Advanced Polymers EpiSpire™ HTS-2401 High Temperature Sulfone Resin
Subcategory: Polysulfone; Thermoplastic
Material Notes: EpiSpire HTS-2401 is a new high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature of 245 °C and HDT of 235 °C, the resin extends the thermal capability range available in other commercially available sulfone polymers (polysulfone, polyethersulfone and polyphenylsulfone). The resin is completely amorphous and fully thermoplastic allowing easy melt fabrication by means of injection molding and other thermoplastic processing techniques. Along with its high thermal performance capabilities, HTS-2401 resin also boasts a long list of high performance attributes which include excellent hydrolytic stability, resistance to acids and bases and inherently flame retardant performance to mention a few. The ease of melt fabrication, coupled with the completely amorphous character assures tight dimensional control during injection molding of precision parts and components. The versatile performance profile of HTS-2401 makes it a good candidate for metal replacement or the replacement of difficult-to-process thermoplastics in a wide range of engineering applications. In its natural state, EpiSpire HTS-2401 resin is transparent with an amber/brown color. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Refractive Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|