Solvay Engineered Polymers DEXFLEX® 777 TPO
Subcategory: Elastomer, TPE; Polypropylene; Thermoplastic
Key Words: Thermoplastic Olefinic Elastomer; Polyolefin
Material Notes: Data provided by Solvay Engineered Polymers.A thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications requiring a combination of high stiffness, good low-temperature impact, and excellent processability. Uses: Claddings, rocker panels, body side moldings, grilles, and other large components requiring durable paintability.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Gardner Impact
- Low Temperature Gardner Impact
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|