Solvay Engineered Polymers DEXFLEX® 870 TPO
Subcategory: Elastomer, TPE; Polypropylene; Thermoplastic
Key Words: Thermoplastic Olefinic Elastomer; Polyolefin
Material Notes: Data provided by Solvay Engineered Polymers.A thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications requiring dimensional stability over a broad temperature range, excellent low-temperature properties and excellent weatherability. Uses: Bumper fascias, air dams, valance panels, sight shields, license-plate brackets, and other injection molded components.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Gardner Impact
- Low Temperature Gardner Impact
- Tear Strength
- CTE, linear 20°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|