Solvay Engineered Polymers DEXFLEX® 1203 TPO
Subcategory: Elastomer, TPE; Polypropylene; Thermoplastic
Key Words: Thermoplastic Olefinic Elastomer; Polyolefin
Material Notes: Data provided by Solvay Engineered Polymers.A thermoplastic olefinic elastomer (TPO) designed for automotive interior applications requiring toughness and excellent colorability. This material is readily processed into injection molded parts and has excellent weatherability. Uses: Scuff plates, A-pillars, and other applications requiring exacting dimensional tolerances for interior applications.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Flexural Modulus
- Gardner Impact
- Low Temperature Gardner Impact
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|