Solvay Engineered Polymers SEQUEL® 1440LS TPO
Subcategory: Polyolefin; Thermoplastic
Material Notes: Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processability, and good paint adhesion. Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Impact Test
- CTE, linear 20°C
|
|
|
|