Solvay Engineered Polymers SEQUEL® 1485 Engineered Polyolefin
Subcategory: Polyolefin; Thermoplastic
Material Notes: Description: SEQUEL® 1485 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, improved scratch and mar resistance, and excellent paintability and processability. Applications: Bumper fascias Information provided by Solvay Engineered Polymers.