Solvay Engineered Polymers SEQUEL® 1823 Engineered Polyolefin
Subcategory: Polyolefin; Thermoplastic
Material Notes: Description: SEQUEL® 1823 engineered polyolefin is designed for automotive exterior applications that require energy management combined with excellent ductility and stiffness over a broad temperature range. This material provides excellent processability and dimensional stability. Applications: Body panels, bumper beams, energy absorbers, and brackets Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Impact Test
- CTE, linear 20°C
|
|
|
|