Solvay Engineered Polymers SEQUEL® 2300 Engineered Polyolefin
Subcategory: Polyolefin; Thermoplastic; Polymer
Material Notes: Description: SEQUEL® 2300 engineered polyolefin is designed for large mold-in-color automotive interior applications that require high stiffness and dimensional stability over a broad temperature range. This material exhibits excellent low-gloss surface appearance and processability. Applications: Instrument panels and components, A and B-pillar covers, and miscellaneous interior trim components that must exhibit high modulus and superior impact performance. Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Filler Content
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Five-Finger Scratch Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|