Solvay Engineered Polymers SEQUEL® E2200 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: SEQUEL® E2200 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require low-temperature toughness and high rigidity. This product is fully colorable and is available in both UV-stabilized and non-UV-stabilized options. It is most functional when used as substrate layer for INDURE® E1500HG to provide a structure with excellent cold temperature impact properties as well as high stiffness. Applications: Substrate layer for E1500HG high gloss cap layer or general purpose monolith material for sheet extrusion and thermoforming. Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Gardner Impact @ 23°C
- Gardner Impact @ -30°C
- Izod Impact, Notched
- Izod Impact, Notched @ -30°C
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|