Solvay Engineered Polymers SEQUEL® E3000 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion-grade material is readily processed into a variety of products and has excellent chemical resistance. This material can be supplied with or without UV stabilizers. Applications: Sheet extrusion and thermoforming Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Gardner Impact @ 23°C
- Gardner Impact @ -30°C
- Izod Impact, Notched
- Izod Impact, Notched @ -30°C
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|