Solvay Engineered Polymers DEXFLEX® B-2020 TPO, Blow Molding Grade
Subcategory: Elastomer, TPE; Polypropylene; Thermoplastic
Key Words: Thermoplastic Olefinic Elastomer; Polyolefin
Material Notes: Data provided by Solvay Engineered Polymers.A thermoplastic olefinic elastomer (TPO) designed for automotive applications in which a balance of stiffness, impact resistance, and processability are important. This blow-molding grade material provides excellent performance properties for interior and underhood parts and, with UV stabilizers, can deliver weatherability appropriate to automotive exterior applications. Uses: General purpose automotive applications.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Flexural Modulus
- Low Temperature Gardner Impact
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|