Solvay Engineered Polymers DEXFLEX® 711 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: DEXFLEX® 711 is a thermoplastic olefinic elastomer compounded with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched) black, and that require very good processing characteristics. Applications: Wheel liners, filler panels, fan shrouds, air dams, and sight shields Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- CTE, linear 20°C
|
|
|
|
| Property Data |