Solvay Engineered Polymers DEXFLEX® 900 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: DEXFLEX® 900 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paintability, and processability. Applications: Bumper fascias, claddings Information provided by Solvay Engineered Polymers
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- CTE, linear 20°C
|
|
|
|
| Property Data |