Solvay Engineered Polymers DEXFLEX® 930 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: DEXFLEX® 930 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact properties at low temperatures, and good paint adhesion. Applications: Bumper fascias and exterior trim Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Impact Test
- CTE, linear 20°C
|
|
|
|