Solvay Engineered Polymers DEXFLEX® 930HS TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: DEXFLEX® 930HS is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact properties at low temperatures, and good paint adhesion. Applications Bumper fascias Information provided by Solvay Engineered Polymers
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Impact Test
- CTE, linear 20°C
|
|
|
|
| Property Data |