Solvay Engineered Polymers DEXFLEX® E160 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: DEXFLEX® E160 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require thermal stability, excellent low-temperature properties, and good dimensional stability over a broad temperature range. This material can be supplied with or without UV stabilizers. Applications: Extrusion and thermoforming or automotive parts, such as luggage racks. Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Gardner Impact @ 23°C
- Gardner Impact @ -30°C
|
|
|
|