Solvay Engineered Polymers DEXFLEX® E756 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toughness. This material is colorable and can be supplies with or without UV stabilizers. Applications: Passenger and roof-mounted air-bag covers that require stiffness and that operate in temperatures ranging from -40°C to 104°C Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Impact Test
- Izod Impact, Notched @ -40°C
- Multi-axial Impact @ -30°C Total Energy
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|