Solvay Engineered Polymers NEXPRENE® 1080A CM/UV Bondable Corner Mold Grades
Subcategory: Elastomer, TPE; Polypropylene; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Material Notes: Description: NEXPRENE® 1080A CM/UV bondable corner mold thermoplastic vulcanizate (TPV) is a fully cross-linked EPDM/PP compound designed to bond to vulcanizate EPDM thermoset elastomers. Applications: NEXPRENE® bondable corner mold grades are designed for corner molding applications that need excellent adhesion to vulcanized EPDM. They are ideal for "glass run channel" weatherseal applications in the automotive market. Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Tear Strength
- Compression Set
- Brittleness Temperature
- Ozone Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|