Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene
Subcategory: Polypropylene; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Material Notes: Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Impact Test
- CTE, linear 20°C
|
|
|
|