Solvay Engineered Polymers INDURE™ X210 TPO
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: INDURE™ X210 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, and processability. Applications: Bumper fascias, cladding. Information provided by Solvay Engineered Polymers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Flexural Modulus
- CTE, linear 20°C
|
|
|
|