Ineos HDPE G60-110
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: Sheet extrusion, thermoforming and large part blow molding
Material Notes: Ineos G60-110 is a high molecular weight, high density polyethylene homopolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding physical performance. Its ASTM D1248 classification is Type IV, Class A, Category 5. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. This resin is Kosher certified.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|