Fortiflex® HDPE HP55-50-155 HDPE Copolymer, High Performance
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: High Density Polyethylene
Material Notes: Fortiflex® HP55-50-155 is a high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in applications requiring a combination of good top load strength and high throughput rate. HP55-50-155 is recommended for use in continuous extrusion blowmolding equipment. This product meets the Food and Drug Administration requirements of CFR 177.1520 for contact with food. This resin is Kosher certified.This product information was provided by Solvay Polymers, now a part of the BP Solvay Polyethylene North America joint venture (Nov. 2001).
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Tensile Impact Strength
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|