Fortiflex® HDPE K44-15-123 HDPE Copolymer with Carbon Black
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: High Density Polyethylene
Material Notes: Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized by the Plastic Pipe Institute as having a PE 3408 rating. The natural version of this resin is available as Fortiflex® K44-15-122.2.5% Carbon Black Concentration This product information was provided by Solvay Polymers, now a part of the BP Solvay Polyethylene North America joint venture (Nov. 2001).
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|